PECVD
Plasma enhanced chemical vapor deposition (PECVD) is performed in a reactor at temperatures up to ~400 degC. The deposited film is a product of a chemical reaction between the source gases supplied to the reactor. A plasma is generated in the reactor to increase the energy available for the chemical reaction at a given temperature. The process is typically performed on one side of the substrate at a time.