| Sides processed |
either |
| Temperature |
25 °C |
| Thickness |
5 .. 8 µm |
| Wafer size |
|
| Equipment |
Headway spinner |
| Equipment characteristics: |
| Batch sizes |
100 mm: 1, 150 mm: 1, 200 mm: 1, 75 mm: 1 |
| Wafer geometry Types of wafers this equipment can accept |
1-flat, 2-flat |
| Wafer holder Device that holds the wafers during processing. |
vacuum chuck |
| Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
glass (category), silicon |
| Wafer thickness List or range of wafer thicknesses the tool can accept |
200 .. 1000 µm |
| Comments: |
|