Lift off

In lift-off processes a sacrificial material, such as photoresist, is first deposited and patterned on the substrate. The material of interest is then deposited on top and the sacrificial material is subsequently removed, leaving behind only the material deposited directly on the substrate. These processes are useful for patterning materials that cannot be etched without affecting underlying materials on the substrate.
Process
ITO lift-off
Platinum lift-off
Tungsten lift-off
Metal lift-off
Lift-off etch (1112A)
Lift-off etch (acetone)
Lift-off