Polyimide Develop (Manual- Durimide) |
|
| Batch size |
1 |
| Depth |
18 .. 75 µm |
| Developer Agent that reacts with masking layer (e.g., photoresist) to etch it selectively. |
HTR- D2 developer |
| Etch type |
wet isotropic |
| Material |
Durimide 7520 |
| Temperature |
20 °C |
| Wafer size |
|
| Equipment |
Wet bench |
| Equipment characteristics: |
| Piece geometry Geometry of wafer pieces the equipment can accept |
rectangular, circular |
| Wafer geometry Types of wafers this equipment can accept |
1-flat, 2-flat |
| Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
quartz (fused silica), silicon carbide, silicon on insulator, quartz (single crystal), sapphire, silicon, Pyrex (Corning 7740), gallium arsenide, indium phosphide |
| Wafer thickness List or range of wafer thicknesses the tool can accept |
250 .. 800 µm |