| Depth |
1.3 .. 25 µm |
| Etch type |
wet isotropic |
| Etchant Solutions and their concentrations. |
AZ300T |
| Material |
photoresist (category) |
| Sides processed |
both |
| Temperature |
90 °C |
| Wafer size |
|
| Equipment |
wet bench (solvent) |
| Equipment characteristics: |
| Batch sizes |
100 mm: 12, 125 mm: 12, 150 mm: 12 |
| MOS clean |
no |
| Piece dimension Range of wafer piece dimensions the equipment can accept |
2 .. 150 mm |
| Piece geometry Geometry of wafer pieces the equipment can accept |
circular, irregular, other, rectangular, triangular shard |
| Piece thickness Range of wafer piece thickness the equipment can accept |
300 .. 1000 µm |
| Wafer geometry Types of wafers this equipment can accept |
1-flat, 2-flat, no-flat, notched |
| Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
Borofloat (Schott), Pyrex (Corning 7740), quartz (fused silica), silicon, silicon on insulator |
| Wafer thickness List or range of wafer thicknesses the tool can accept |
300 .. 1000 µm |