on front I-line exposure (MJB3) |
|
| Feature geometry Shape of feature with dimensions characterized by the minimum feature size |
line |
| Field geometry Shape of field with dimensions characterized by the maximum field size |
circle |
| Material |
photoresist (category) |
| Min feature size |
1 µm |
| Sides processed |
either |
| Wafer size |
|
| Equipment |
Karl Suss MJB3 Mask Aligner |
| Equipment characteristics: |
| Wafer geometry Types of wafers this equipment can accept |
no-flat, 1-flat, 2-flat, notched |
| Wafer holder Device that holds the wafers during processing. |
vacuum chuck |
| Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
glass (category), Pyrex (Corning 7740), quartz (single crystal), silicon, silicon on insulator |
| Wafer thickness List or range of wafer thicknesses the tool can accept |
100 .. 500 µm |