Acid bench |
|
|---|---|
| Model | |
| Type | commercial |
| Equipment Characteristics | |
| Batch sizes | 100 mm: 25, 150 mm: 25 |
| MOS clean | no |
| Wafer diameter(s) List or range of wafer diameters the tool can accept |
100 mm, 150 mm |
| Wafer geometry Types of wafers this equipment can accept |
1-flat, 2-flat, no-flat, notched |
| Wafer holder Device that holds the wafers during processing. |
teflon boat |
| Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
alumina, BK7, Borofloat (Schott), ceramic, Foturan (Schott), fused silica, glass (Hoya), glass-ceramic, quartz (fused silica), quartz (single crystal), silicon, silicon on insulator |
| Wafer thickness List or range of wafer thicknesses the tool can accept |
200 .. 750 µm |