Post-exposure bake oven

Model
Type
Equipment Characteristics
Wafer diameter(s)
List or range of wafer diameters the tool can accept
100 mm, 150 mm, 200 mm
Wafer holder
Device that holds the wafers during processing.
cassette
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
silicon, glass (category), quartz (single crystal), gallium arsenide, silicon on insulator, silicon on sapphire
Wafer thickness
List or range of wafer thicknesses the tool can accept
200 .. 1000 µm