Gryphon Sputtering System

Gryphon Sputtering System

Model
Type
Equipment Characteristics
Wafer diameter(s)
List or range of wafer diameters the tool can accept
100 mm
Wafer holder
Device that holds the wafers during processing.
palette
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
silicon, quartz (single crystal), silicon on insulator
Wafer thickness
List or range of wafer thicknesses the tool can accept
300 .. 600 µm