logo
Denton Discovery 24

Denton Discovery 24

Model
Type
Equipment Characteristics
Batch sizes 100 mm: 1, 150 mm: 1
Wafer diameter(s)
List or range of wafer diameters the tool can accept
100 mm, 150 mm
Wafer holder
Device that holds the wafers during processing.
stainless steel
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
alumina, Borofloat (Schott), silicon, silicon dioxide
Wafer thickness
List or range of wafer thicknesses the tool can accept
300 .. 1000 µm