Tylan Furnace (Boron diffusion, Tube #5) |
|
|---|---|
| Model | |
| Type | commercial |
| Equipment Characteristics | |
| Wafer diameter(s) List or range of wafer diameters the tool can accept |
75 mm, 100 mm |
| Wafer geometry Types of wafers this equipment can accept |
no-flat, 1-flat, 2-flat |
| Wafer holder Device that holds the wafers during processing. |
quartz boat |
| Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
silicon, silicon on insulator |
| Wafer thickness List or range of wafer thicknesses the tool can accept |
300 .. 600 µm |
| Attachments | |