logo
KLA-Tencor P-15 stylus profilometer

KLA-Tencor P-15 stylus profilometer

Model P-15
Type commercial
Equipment Characteristics
Batch sizes 100 mm: 1, 150 mm: 1, 50 mm: 1, 75 mm: 1
Wafer diameter(s)
List or range of wafer diameters the tool can accept
50 mm, 75 mm, 100 mm, 150 mm
Wafer geometry
Types of wafers this equipment can accept
1-flat, 2-flat, notched, no-flat
Wafer holder
Device that holds the wafers during processing.
aluminum plate
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
quartz (fused silica), gallium arsenide, silicon
Wafer thickness
List or range of wafer thicknesses the tool can accept
200 .. 800 µm
Attachments