Process Hierarchy

  Epoxy bonding (air, with alignment)
Alignment type
Method used to align materials to be bonded.
optical
Ambient
Ambient to which substrate is exposed during processing
air
Duration 120 min
Pressure
Pressure of process chamber during processing
1 atm
Temperature 120 °C
Wafer size
Wafer size
Equipment Wafer bonder
Equipment characteristics:
Batch sizes 100 mm: 2, 25 mm: 2, 50 mm: 2, 75 mm: 2
MOS clean no
Wafer geometry
Types of wafers this equipment can accept
1-flat, 2-flat, no-flat, notched
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
Borofloat (Schott), Pyrex (Corning 7740), silicon
Wafer thickness
List or range of wafer thicknesses the tool can accept
300 .. 1000 µm