logo
Photoresist coat (950 PMMA 4 A in anisole): View
Process Hierarchy
Bonding
Clean
Consulting
Deposition
   Evaporation
   LPCVD
   Low-stress SiN deposition
   Miscellaneous deposition
   Oxidation
   PECVD
   Spin casting
   Sputtering
Doping
Etch
LIGA
Lift off
Lithography
Mask making
Metrology
Miscellaneous
Packaging
Polishing
Process technologies
Thermal
Unique capabilities
on front
  Photoresist coat (950 PMMA 4 A in anisole)
Batch size 1
Material PMMA
Microstructure amorphous
Sides processed either
Thickness 2000 .. 4000 Å
Wafer size
Wafer size
Equipment Solitec 5100
Equipment characteristics:
Wafer holder
Device that holds the wafers during processing.
vacuum chuck
Wafer materials
List of wafer materials this tool can accept (not list of all materials, just the wafer itself).
silicon, glass (category)
Wafer thickness
List or range of wafer thicknesses the tool can accept
200 .. 800 µm
Comments:
  • This is a positive tone resist used for E-Beam, Deep UV (200-250nm), and X-Ray Lithographic process.