| Material |
HMDS |
| Setup time |
30 min |
| Sides processed |
both |
| Temperature |
120 °C |
| Wafer size |
|
| Equipment |
Yield Vacuum Vapor Prime System (Model YES-5) |
| Equipment characteristics: |
| Wafer geometry Types of wafers this equipment can accept |
1-flat, 2-flat |
| Wafer holder Device that holds the wafers during processing. |
teflon cassette |
| Wafer materials List of wafer materials this tool can accept (not list of all materials, just the wafer itself). |
silicon |
| Wafer thickness List or range of wafer thicknesses the tool can accept |
300 .. 700 µm |